enLanguage
TDI Polyurethane Prepolymer
video
TDI Polyurethane Prepolymer

TDI Polyurethane Prepolymer

TDI polyurethane prepolymer
Good liquidity
Easy to use
Fast demoulding
High yield
Send Inquiry
Description

TDI polyurethane prepolymer produced by Shandong XinRuiTuo Precision Industry Co., Lted. is a high-end product. After the product is formed, it has the remarkable characteristics of wear resistance, oil resistance, vibration absorption, solvent resistance, high mechanical strength, tensile resistance and tear resistance.

 

flexible polyurethane casting resin

 

Our company has been engaged in TDI, MDI, PPDI, ND and other high-tech elastomer industries since 2006. From the beginning, we have been committed to the R&D, production and sales of TDI polyurethane prepolymer. After a period of accumulation, we have not only broadened the product line, but also improved the product quality step by step. We firmly believe that quality determines the fate of a production-oriented company. After so many years of development, with our rich experience, professional technology and national influence in the polyurethane industry, more manufacturers from home and abroad have learned about the advantages and benefits of high-quality polyurethane elastomers.

 

We have various types of TDI polyurethane prepolymers, please refer to the following table for details:

  • Polyester T100 type prepolymer:

     

Model

1022

1026

1030

1036

1042

1050

1055

1060

NCO content %

2.2±0.2

2.6±0.2

3.0±0.2

3.6±0.2

4.2±0.2

5.0±0.2

5.5±0.2

6.0±0.2

State of matter at 20°C

white solid

white solid

white solid

white solid

white solid

white solid

white solid

white solid

Hardener

MOCA

MOCA

MOCA

MOCA

MOCA

MOCA

MOCA

MOCA

100g prepolymer curing agent dosage (g)

6.5

7.7

8.8

10.6

12.4

14.8

16.2

17.7

Prepolymer/curing agent mixing temperature (°C)

85/120

85/120

85/120

80/120

80/120

80/120

75/120

75/120

Viscosity at 85°C (mpa·s)

3000

2600

2000

1600

1300

1100

1000

900

Gel time (min)

15-20

14-18

12-16

10-15

8-13

6-10

5-9

4-8

Post curing time (100℃/h)

16

16

16

16

16

16

16

16

Hardness (Shore A)

70±2

75±2

80±2

85±2

90±2

92±2

94±2

96±2

Tensile strength (mpa)

42

43

45

46

46

47

49

50

100% modulus stress (mpa)

2.5

3.5

3.7

4.1

6

8

10

12

300% modulus stress (mpa)

4

5.5

7

8

12

16

20

25

Elongation at break (%)

850

720

680

660

550

500

480

460

Right Angle Tear Strength (kN/m)

50

58

72

80

92

105

118

125

Pants tear strength (kN/m)

18

22

32

40

45

46

48

50

Rebound (%)

43

40

38

35

34

32

30

28

Density at 25°C (g/cm3)

1.23

1.24

1.25

1.25

1.25

1.25

1.26

1.26

DIN wear (cm3)

40

42

42

43

43

45

46

49

Acron wear(cm3)

0.025

0.023

0.023

0.022

0.022

0.021

0.021

0.02

 

  • Polyester T80 type prepolymer:

    Model

    8025

    8030

    8035

    8042

    8045

    8049

    8055

    8060

    NCO content %

    2.5±0.2

    3.0±0.2

    3.5±0.2

    4.2±0.2

    4.5±0.2

    4.9±0.2

    5.5±0.2

    6.0±0.2

    State of matter at 20°C

    white solid

    white solid

    white solid

    white solid

    white solid

    white solid

    white solid

    white solid

    Hardener

    MOCA

    MOCA

    MOCA

    MOCA

    MOCA

    MOCA

    MOCA

    MOCA

    100g prepolymer curing agent dosage (g)

    7.4

    8.8

    10.3

    12.4

    13.3

    14.5

    16.2

    17.7

    Prepolymer/curing agent mixing temperature (°C)

    85/120

    85/120

    80/120

    80/120

    80/120

    80/120

    80/120

    80/120

    Viscosity at 85°C (mpa·s)

    3000

    2400

    2000

    1500

    1400

    1200

    1000

    900

    Gel time (min)

    6-10

    4-8

    4-7

    3-5

    2-5

    2-4

    1-3

    1-2

    Post curing time (100℃/h)

    16

    16

    16

    16

    16

    16

    16

    16

    Hardness (Shore A)

    75±2

    80±2

    85±2

    90±2

    91±2

    93±2

    95±2

    97±2

    Tensile strength (mpa)

    42

    44

    48

    49

    48

    50

    52

    55

    100% modulus stress (mpa)

    3

    4

    5

    8

    8

    9

    11

    15

    300% modulus stress (mpa)

    6

    7

    10

    13

    15

    18

    20

    30

    Elongation at break (%)

    760

    740

    680

    630

    550

    480

    460

    400

    Right Angle Tear Strength (kN/m)

    60

    62

    80

    100

    105

    110

    120

    135

    Pants tear strength (kN/m)

    23

    26

    37

    45

    47

    50

    58

    65

    Rebound (%)

    42

    40

    38

    30

    29

    25

    23

    28

    Density at 25°C (g/cm3)

    1.23

    1.23

    1.24

    1.25

    1.26

    1.26

    1.27

    1.28

    DIN wear (cm3)

    40

    41

    42

    42

    43

    45

    43

    42

    Acron wear(cm3)

    0.025

    0.024

    0.024

    0.023

    0.024

    0.023

    0.021

    0.02

     

  • Polyether T100 type prepolymer & Polyether T80 type prepolymer:

Model

1145

1155

1165

8130

8135

8143

8151

NCO content %

4.5±0.2

5.5±0.2

6.5±0.2

3.0±0.2

3.5±0.2

4.3±0.2

5.1±0.2

State of matter at 20°C

colorless transparent liquid

colorless transparent liquid

colorless transparent liquid

colorless transparent liquid

colorless transparent liquid

colorless transparent liquid

colorless transparent liquid

Hardener

MOCA

MOCA

MOCA

MOCA

MOCA

MOCA

MOCA

100g prepolymer curing agent dosage (g)

13.3

16.2

19.2

8.8

10.3

12.7

15.0

Prepolymer/curing agent mixing temperature (°C)

80/120

80/120

75/120

80/120

80/120

80/120

75/120

Viscosity at 85°C (mpa·s)

350

300

270

350

330

350

360

Gel time (min)

10

8

6

6-10

4-7

3-6

2-5

Post curing time (100℃/h)

16

16

16

16

16

16

16

Hardness (Shore A)

85±2

90±2

95±2

73±2

80±2

85±2

90±2

Tensile strength (mpa)

25

30

35

8

11

20

32

100% modulus stress (mpa)

6

7

10

2

3

6

9

300% modulus stress (mpa)

10

11

16

5

6

11

15

Elongation at break (%)

500

430

380

650

550

480

420

Right Angle Tear Strength (kN/m)

60

85

95

35

45

60

85

Pants tear strength (kN/m)

18

20

25

9

15

18

28

Rebound (%)

27

25

22

48

43

38

30

Density at 25°C (g/cm3)

1.10

1.12

1.18

1.08

1.09

1.11

1,14

DIN wear (cm3)

120

115

110

130

125

116

105

Acron wear(cm3)

0.05

0.048

0.046

0.05

0.048

0.055

0.052

 

https://youtube.com/shorts/iRIGehzjIp4?si=LBMgCyK1A6JnNlXc

If there is any data in the product specification that has not been updated in time, please contact me, we will be very grateful. Our company produces TDI Polyurethane Prepolymer and other series of products in large quantities all the year round. We have new products that have not been updated in time. If the product you need does not appear in the above details, please contact me.

 

 

 

Why choose us?

  • We use only the best materials in the manufacturing process.
  • Continuous pursuit of innovation, progress, and strive to be perfect, to provide customers with quality service, is the source of consumer trust.
  • We are dedicated to improving the quality of our products through ongoing research and development.
  • We adhere to the corporate culture spirit of independence, cooperation, marketization, and upward gratitude, and use high-quality products to benefit customers and achieve employees.
  • You can rely on us to provide you with fast and efficient solutions for your casting needs.
  • We accelerate the pace of international operation and strive to enhance the international reputation of our company.
  • We offer a range of custom solutions to meet the specific needs of our clients.
  • We continue to strengthen internal management, reinforce group control, and accelerate the adjustment of institutional mechanisms.
  • We have a deep understanding of the material properties and manufacturing techniques used in our products.